Interfacial Chemistry of Layered Oxide Cathodes for Sodium-Ion Batteries: A Review

Caixia Chen1, Peizhao Shan1, Jun Zhou1, Chenpeng Xie1, Yixiao Li1, Zhongru Zhang1, Wenhua Zuo1, Yong Yang1,2   

  1. 1. State Key Lab for Physical Chemistry of Solid Surfaces, College of Chemistry and Chemical Engineering, Xiamen University, Xiamen 361005, Fujian, China;
    2. College of Energy, Xiamen University, Xiamen 361005, Fujian, China
  • Received:2025-12-09 Revised:2026-05-10 Accepted:2026-06-18 Online:2026-09-20 Published:2026-10-19
  • Supported by:
    This work was supported by the Commanding Heights of Science and Technology of Chinese Academy of Science (No. LDES15 0000), Regional Development Project of Fujian Province (No. 2022H4010) and Xiamen Major Science and Technology Plan Project (Future Industry Field) (No. 3502Z20231059).

Abstract: Sodium-ion batteries (SIBs) represent a compelling alternative to lithium-ion batteries (LIBs) for large-scale industrialization, primarily due to their cost-effectiveness, enhanced safety profiles, and superior performance in cold climates. Within the spectrum of cathode materials, sodium-based layered transition-metal oxides (NaxTMO2) stand out for their high energy density and manufacturing scalability. Nevertheless, practical deployment is severely impeded by surface and interfacial instabilities triggered by environmental exposure and electrolyte interactions. This paper offers a comprehensive review of the interfacial instability mechanisms in NaxTMO2, encompassing their origins, evolutionary pathways, mitigation strategies, and cutting-edge characterization techniques. We begin by elucidating the fundamental thermodynamics and kinetics governing surface and interfacial behaviors, demonstrating how the coupling of bulk and interface evolution induces structural degradation and capacity decay. Subsequently, we systematically classify stabilization strategies—including bulk-phase engineering, interfacial architecture design, and electrolyte optimization—evaluating their efficacy in addressing specific failure modes. The critical roles of in situ and operando characterization in decoding interfacial evolution under coupled electrochemical, mechanical, and chemical stresses are also analyzed. Finally, we propose future research directions for interface stabilization, highlighting the imperative to translate fundamental insights into actionable design principles for SIBs and next-generation energy storage systems.

Key words: Sodium-ion batteries, Layered oxide cathodes, Interfacial chemistry, Modification strategies, Interface characterization